ERYONE Silk PLA Filament 1KG Silk 2.2LBS 1.75mm 3D Printer Filament for FDM Printers Glossy Rich Colours

£24.95

Color

Silk Copper Silk White Silk Blue Silk Emerald Green Silk Pink Silk Gold Silk Silver

Material

PLA Silk

ERYONE Silk PLA Filament 1KG Silk 2.2LBS 1.75mm 3D Printer Filament for FDM Printers Glossy Rich Colours

£24.95

Color

Silk Copper Silk White Silk Blue Silk Emerald Green Silk Pink Silk Gold Silk Silver

Material

PLA Silk
Ships from our: UK Warehouse

Estimated delivery 4 to 7.

Delivery to the UK only
Product description

ERYONE Silk PLA Filament is a high quality PLA Filament, ideal for making parts and models with a high gloss shine. It produces models with a very high gloss finish, brighter than most other silk filaments.

Suits most 3D Printers from Creality 3D, Artillery, SUNLU, Geeetech, XVICO, Eaythreed and more. 

Degradable and environmentally friendly, ERYONE filament is made from eco-friendly corn starch and the PLA itself can be recycled.

Features:

  • Silk Texture: Extremely fine and smooth on the print surface.
  • Stable Printing: Neatly rolled, high quality.
  • Little Clogging: The diameter is strictly controlled at 1.75±0.03mm.
  • Professional Packaging, Vacuumed Sealed: ERYONE filament is supplied in a sealed vacuum bag with a desiccant bag, keeping it dry and free from dust and foreign particles, prevent nozzle jams and yield smooth 3D models.
  • High Compatibility: Compatible with 3D Printers and 3D Pens that use 1.75MM filament, Such as: Prusa, Makerbot,etc. Our filaments had been tested on various brands of 3D printer in the market and with positive customers' feedback.

Specifications:

  • Filament Diameter: 1.75mm
  • Finish: Gloss Silk
  • Tolerance: ± 0.03mm
  • Print Temperature: 195-215°C
  • Recommended Print Speed: 30-60mm/s
  • Heated Bed Temp: 55-70°C
  • Gross weight: 1.35kg (approx)
  • Net Weight: 1kg (approx)

FAQ:

  • Clogging: Clogging is caused by uneven wire diameter or too low a temperature. Clean the nozzle before use and raise the temperature to reduce the chance of clogging.
  • Stringing: If the temperature is too high, the flow of PLA is too fast, or the feed parameters are not set properly, wire stringing will be caused. Reducing the temperature and speed corrections will solve these issues.
  • Over Extrusion: Too high a temperature, too slow speed, or nozzle diameter in the section does not match will cause too much extruding at the nozzle outlet, and there will be residual material.

Customer Reviews

Based on 4 reviews Write a review
Previous Product Next Product

Free Tracked Shipping*

*Some countries may have a small delivery charge due to disproportionately high shipping.

Fully secured payments

All our payments are handled by secure methods, we'll never see or ask for your payment details.

Friendly service

We pride ourselves on great service, no matter the order value, we want you to be satisfied with it.