ERYONE CERPRiSE Standard PLA Filament For 3D Printing 1.75mm Filament ± 0.03mm Tolerance 1kg Spool

£18.99 £13.99 35% OFF

Color

Red White Blue Green Black Grey

Material

PLA

ERYONE CERPRiSE Standard PLA Filament For 3D Printing 1.75mm Filament ± 0.03mm Tolerance 1kg Spool

£18.99 £13.99

Color

Red White Blue Green Black Grey

Material

PLA
Ships from our: UK Warehouse

Estimated delivery 4 to 7.

Delivery to the UK only
Video ERYONE CERPRiSE Standard PLA Filament For 3D Printing 1.75mm Filament ± 0.03mm Tolerance 1kg Spool
Product description

ERYONE CERPRiSE PLA Filament is a high quality PLA Filament, made from virgin plastic and with strong colours, supplied in vacuum packaging for freshness. Wound to prevent tangles, tight tolerance control and quality material ensures great prints every time. Suits most FDM 3D Printers from Creality 3D, Artillery, SUNLU, Geeetech, XVICO, Eaythreed and more.

Quality is at the heart of ERYONE, Founded in 2018, Headquartered in Shenzhen, the heart of Chinese Electronics, ERYONE benefits from direct access to raw material suppliers and young talent.

Features:

  • Minimum Tolerance | Low Warping | Ensure Consistent Feeding and Stable Prints
    Minimum tolerance and low warping to ensure consistent feeding and stable prints, No clogging, extremely high successful rate, resulting in printed parts that have an outstanding surface finish and are highly precise.
  • Purest-grade Material | Made in USA | Non Toxic and Limited Smell
    ERYONE filaments are 100% Made in the USA with virgin materials, Biodegradable and Eco-friendly, NO harm to user and environment. Ideal for indoor printing.
  • Professional Packaging | Vacuumed Sealed
    ERYONE is supplied in a sealed vacuum bag with a desiccant bag to keep it dry and keep out dust and foreign particles, prevent nozzle jams and yield smooth 3D models.
  • High Compatibility
    Compatible with 3D Printers and 3D Pens that use 1.75MM filament, Such as:Prusa,Makerbot,etc. Our filaments had been tested on various brands of 3D printer in the market and with positive customers' feedback.

Specifications:

  • Filament Diameter: 1.75mm
  • Tolerance: ± 0.03mm
  • Print Temperature: 190-220°C
  • Recommended Print Temperature: 210-220°C
  • Recommended Print Speed 40-60mm/s
  • Produced mainly from Corn Starch, eco friendly material.
  • Net Weight: 1kg (inc spool)
  • Gross Weight: 1.3-1.4kg

Common 3D Printers Recommended Settings

Make/Model

Extruder Type/Heated Bed Type

Settings

Creality Ender 3

Bowden/Flexible Bed Sticker

Printing Temperature: 210-220°C

Heated Bed Temperature: 55-65°C

Printing Speed: 30-45mm/s

Retracting Length: 2-4mm

Retracting Speed: 60-100mm/s

Creality CR-10

Bowden/Glass Bed

Printing Temperature: 210-220°C

Heated Bed Temperature: 65-70°C

Printing Speed: 30-45mm/s

Retracting Length: 2-5mm

Retracting Speed: 80-110mm/s

 

 

Anycubic Mega-S

 

Bowden/ Microporous Coating Glass Bed

Printing Temperature: 210-220°C

Heated Bed Temperature: 60-70°C

Printing Speed: 30-45mm/s

Retracting Length: 2-4mm

Retracting Speed: 70-100mm/s

Prusa i3

Direct Drive Extruder/PEI Bed Sticker

Printing Temperature: 200-220°C

Heated Bed Temperature: 55-70°C

Printing Speed: 30-50mm/s

Retracting Length: 0.8mm

Retracting Speed: 30-40mm/s

Eryone Thinker S

Bowden/PEI Bed Sticker

Printing Temperature: 210-220°C

Heated Bed Temperature: 55-70°C

Printing Speed: 30-45mm/s

Retracting Length: 4mm

Retracting Speed: 90-110mm/s

Eryone Thinker SE

Bowden/Glass Bed

Printing Temperature: 210-220°C

Heated Bed Temperature: 65-70°C

Printing Speed: 30-45mm/s

Retracting Length: 4mm

Retracting Speed: 80-110mm/s

Eryone Thinker ER-20

Bowden/Silk-Screen Glass Bed

Printing Temperature: 210-220°C

Heated Bed Temperature: 60-70°C

Printing Speed: 30-50mm/s

Retracting Length: 2-5mm

Retracting Speed: 80-110mm/s


FAQ:

  • Clogging: Clogging is caused by uneven wire diameter or too low a temperature. Clean the nozzle before use and raise the temperature to reduce the chance of clogging.
  • Stringing: If the temperature is too high, the flow of PLA is too fast, or the feed parameters are not set properly, wire stringing will be caused. Reducing the temperature and speed corrections will solve these issues.
  • Over Extrusion: Too high a temperature, too slow speed, or nozzle diameter in the section does not match will cause too much extruding at the nozzle outlet, and there will be residual material.

Free Tracked Shipping*

*Some countries may have a small delivery charge due to disproportionately high shipping.

Fully secured payments

All our payments are handled by secure methods, we'll never see or ask for your payment details.

Friendly service

We pride ourselves on great service, no matter the order value, we want you to be satisfied with it.